Oġġett | ErNiCrMo-3 | ErNiCrMo-4 | ErNiCrMo-13 | ErNiCrFe-7 | ErNiCr-3 | ErNiCrCu-7 | ErCuNi | ErNi-1 |
C | 0.1 | 0.02 | 0.01 | 0.04 | 0.1 | 0.15 | 0.03 | 0.15 |
Mn | 0.05 | 1 | 0.5 | 1 | 2.5-3.5 | 4 | 0.5-1.0 | 1 |
Fe | 5 | 4-7 | 1.5 | 7-11 | 3 | 2.5 | 0.65 | 1 |
P | 0.02 | 0.04 | 0.015 | 0.02 | 0.03 | 0.02 | 0.01 | 0.03 |
S | 0.015 | 0.03 | 0.005 | 0.015 | 0.015 | 0.015 | 0.01 | 0.015 |
Si | 0.05 | 0.08 | 0.1 | 0.5 | 0.5 | 1.25 | 0.15 | 0.75 |
Cu | 0.5 | 0.5 | N/A | 0.3 | 0.5 | mistrieħ | mistrieħ | 0.25 |
Ni | ≥58 | mistrieħ | mistrieħ | mistrieħ | ≥67 | 62-69 | 30-32 | ≥93 |
Co | N/A | 2.5 | 0.3 | N/A | N/A | N/A | N/A | N/A |
Al | 0.4 | N/A | 0.1-0.4 | 1.1 | N/A | 1.25 | 0.15 | 1.5 |
Ti | 0.4 | N/A | N/A | 1 | 0.75 | 1.5-3 | 0.5 | 2-3.5 |
Cr | 20-23 | 14.5-16.5 | 22-24 | 28.5-31 | 18-22 | N/A | N/A | N/A |
Nb+Ta | 3.5-4.15 | N/A | 1.8-2.5 | 0.01 | 2-3 | N/A | N/A | N/A |
Mo | 8-10 | 15-17 | 15-16 | 0.5 | N/A | N/A | N/A | N/A |
V | N/A | 0.35 | N/A | N/A | N/A | N/A | N/A | N/A |
W | N/A | 3-4.5 | N/A | N/A | N/A | N/A | N/A | N/A |
Mistrieħ | ≤0.5 | ≤0.5 | ≤0.5 | ≤0.5 | ≤0.5 | ≤0.5 | ≤0.5 | ≤0.5 |
Tip | Standard | Kompożizzjoni kimika tal-manin % | Applikazzjoni tipika |
Wajer tal-welding tan-nikil | A5.14 ERNi-1 | Ni ≥ 93 Ti3 Al1 Cr– Mo– | ERNi-1 jintuża għall-iwweldjar GMAW, GTAW u ASAW ta' Nikil 200 u 201, li jgħaqqad dawn il-ligi ma' azzar li ma jissaddadx u karbonju, u metalli bażiċi oħra tan-nikil u tar-ram-nikil. Użat ukoll għall-overlaying azzar. |
Wajer NiCuwelding | A5.14 ERNiCu-7 | Ni 65 Cr– Mo– Ti2 Oħrajn: Cu | ERNiCu-7 huwa wajer bażi ta 'liga tar-ram-nikil għall-iwweldjar GMAW u GTAW ta' ligi Monel 400 u 404. Użat ukoll għall-kisi ta 'azzar wara l-ewwel applikazzjoni Saff ta '610 nikil. |
Wajer tal-welding CuNi | A5.7 ERCuNi | Ni 30 Cr– Mo– Oħrajn: Cu | ERCuNi jintuża għall-iwweldjar bl-ark tal-metall tal-gass u tat-tungstenu tal-gass. Jista 'jintuża wkoll bl-iwweldjar oxy-fuel ta' 70/30, 80/20, u 90/10 tar-ram ligi tan-nikil. Saff ta 'barriera ta' liga tan-nikil 610 huwa rrakkomandat qabel l-azzar overlaying bil-proċess ta 'weldjatura GMAW. |
NiCr wajer tal-welding | A5.14 ERNiCrFe-3 | Ni≥ 67 Cr 20 Mo— Mn3 Nb2.5 Fe2 | L-elettrodi tat-tip ENiCrFe-3 jintużaw għall-iwweldjar ta’ ligi tan-nikil-kromju-ħadid għalihom infushom u għall-iwweldjar differenti bejn ligi tan-nikil-kromju-ħadid u azzar jew azzar li ma jissaddadx. |
A5.14 ERNiCrFe-7 | Ni: Mistrieħ Cr 30 Fe 9 | It-tip ERNiCrFe-7 jintuża għall-iwweldjar bl-ark tal-gass-tungstenu u l-ark tal-metall tal-gass ta 'INCONEL 690. | |
Wajer tal-iwweldjar NiCrMo | A5.14 ERNiCrMo-3 | Ni≥ 58 Cr 21 Mo 9 Nb3.5 Fe ≤1.0 | ERNiCrMo-3 jintuża primarjament għat-tungstenu tal-gass u l-ark tal-metall tal-gass u l-metalli bażiċi tal-kompożizzjoni li jaqblu. Jintuża wkoll għall-iwweldjar Inconel 601 u Incoloy 800. Jista 'jintuża biex iwweldja kombinazzjonijiet differenti tal-metall bħall-azzar, l-istainless steel, Inconel u Ligi Incoloy. |
A5.14 ERNiCrMo-4 | Ni Rest Cr 16 Mo 16 W3.7 | ERNiCrMo-4 jintuża għall-iwweldjar ta 'materjali bażi tan-nikil-kromju-molibdenu għalih innifsu, azzar u ligi oħra ta' bażi tan-nikil u għal azzar tal-kisi. | |
A5.14 ERNiCrMo-10 | Ni Rest Cr 21 Mo 14 W3.2 Fe 2.5 | ERNiCrMo-10 jintuża għall-iwweldjar ta 'materjali bażi tan-nikil-kromju-molibdenu għalihom infushom, azzar u ligi oħra ta' bażi tan-nikil, u għall-kisi tal-azzar. Jista 'jintuża biex iwweldja azzar inossidabbli duplex, super duplex. | |
A5.14 ERNiCrMo-14 | Ni Rest Cr 21 Mo 16 W3.7 | ERNiCrMo-14 jintuża għall-iwweldjar tal-gass-tungstenu-ark u tal-gass-metall-ark ta 'azzar inossidabbli duplex, super-duplex u super-awstenitiku, kif ukoll ligi tan-nikil bħal UNS N06059 u N06022, liga INCONEL C-276, u ligi INCONEL 22, 625, u 686. |